Secrets to repairing welding defects in thin-walled hollow sections
@Scarlett6zj3285 Follower
695.945 Aufrufe
19 Kommentare
Kommentare aus dem Originalbeitrag auf X (Twitter)

@uncle_b12
Looks like shit
61 Likes

@keanu_keen
You’re doing good up until you start welding and then downhill as fast as possible 🤧
21 Likes

@juanchis1309
Chimbo ese trabajo pésimo la soldadura no puede quedar así de montada mal soldador
9 Likes

@ZRMD123
Should’ve blunted that edge. Imagine someone runs into that knife!
6 Likes

@A_Wil24
That looks horrible. 🫣
5 Likes

@Maicle16
Предупреждай когда варить начинаешь! Зайцев нахватался, блятть из-за вас!

@RugerJH22
Tf I don’t very do to you?

@KnightWingStyle
The best welds you cant see

@vermuir10470
Next you should learn how to weld.

@AirezHent
Nice holes in the weld

@shinobi1776
Now, hit that bitch with a tiger paw.

@Minischwanzlos2
So schlecht das es weh tut beim zu sehen

@BeefLoMein93
Hell yeah dude this shit was sick

@1997slucky
Senin yapacağın kaynağı sikim tek seferde git amk nakış gibi yap bu ne aq sıra dağı gibi

@SlenderSkeptic
what on earth was secret about this?

@junxfff
Muy mal correlo a ese soldador rata

@Sir_PeteShiffy
Dog shit

@HuskyHaulerZR2
Shits not gonna pass ndt

@Marciio_Ramos
Fez sinal de não com dedo, infelizmente.. próximo!